Potassium chloride fineDepending on the mode to process the rock sylvinite ore by different methods - floatation method and hot-leaching method
Depending on the treatment mode - with the reagents, anti-caking agents and dust-suppression agents - non-dusty, dust-free, standard.
Chemical composition:
K2O - not less than 60%
H20- no more than 0,5%
Dustiness - no more than 0,2 g/kg

Potassium chloride granular
Depending on the mode to process the rock sylvinite -floatation method and hot-leaching method
It is also treated with the reagents,and dust-suppression agents.
Chemical composition:
K2O - not less than 60%
H20 - no more than 0,5%
Dustiness - no more than 0,2 g/kg
Granulometric composition/mass portion of fractions:
more than 4 mm - no more than 3%
from 2 mm up to 4 mm - not less than 87%
Dynamic strength - 85%
Friability- 100%
Dustiness - no more than 0,05 g/kg

Potassium chloride technical
Depending on the mode to process the sylvinite - hot-leaching method, treating with reagents and anti-caking reagents is possible.
Chemical composition:
K2O - not less than 62%
H20 - no more than 0,2%
Friability - 100 %

Sodium chloride technical - mineral concentrate (halite) Grades A,B,C
NaCI - not less than 98% (A), 97% (B), 94%(C)
H20 - no more than 0,7% (A,B)

Common edible rock salt - 1st grade
NaCI - not less than 97,7%
H20- no more than 0,25%
Granulometric composition: grind N2
Up to 2,5 mm inclusive - not less than 90%
Over 4,5 mm - no more than 5%

Common edible rock salt iodized
Chemical composition:
NaCI - not less than 97,7%
H20 - no more than 0,25%
Granulometric composition: grind No.1
Up to 2,5 mm inclusive - not less than 85%
Over 2,5 mm - no more than 3%

Common feeding salt
Chemical composition:
NaCI - not less than 95%
H20 - no more than 0,5%